Acrylic sports courts in Tanzania.

A specialized base adhesive, an acrylic mid-layer and a wear-resistant acrylic surface layer. The elastic version builds 5 mm of coarse and fine acrylic elastic coats.

Supplied by Sahihi Construction Chemicals, ordered per job, ready in 3 to 5 days.

Oriental Yuhong's drawing of the acrylic court layers, a tennis court on top

Where it goes

For tennis courts, low-cost outdoor basketball courts, lightweight rooftop courts and gym equipment areas. On asphalt or concrete only.

  • Durability
  • Rebound
  • Load-bearing

Also called acrylic sports court, hard or elastic.

The build-up

Pull the acrylic court apart.

A labelled diagram, not to scale.

The layers, top to bottom

PSV-701/702 sports field marking paint.

Turned it, pulled it apart? Ask us for it.

Materials

What your area takes.

Build-up and base

Common court sizes. Measure your own site.

Materials for Acrylic court, Hard acrylic, concrete base, 608 m²
ProductLayerQuantityPacks
PSV Acrylic PrimerBase primer213 kg5 × 50 kg
PSV-108 AdhesiveBase primer91.2 kg2 × 50 kg
Cement, 42.5 gradeBought locallyBase primer365 kg-
Quartz sandBought locallyBase primer243 kg-
PSV Acrylic Topcoat, red, green or blueTopcoat243 kg10 × 25 kg
Quartz sand (200 mesh)Topcoat182 kg4 × 50 kg
PSV Acrylic Line Marking PaintLine marking6.1 kg2 × 4 kg

From Oriental Yuhong's consumption per m², without waste. Porous asphalt takes more primer, so check on site. A guide, not a quotation.

How it is built

The stages, and the site.

  1. 01Foundation construction
  2. 02Primer coating
  3. 03Intermediate coating
  4. 04Interface layer
  5. 05Surface layer
  6. 06Marking
  • Concrete of C25 strength, solid, with no laitance or dusting, cured at least 28 days for silicon PU and 20 days for acrylic.
  • A fall of 0.5 to 0.7% so the court drains. Under a 3 m straightedge, water less than 3 mm deep, at 90% of the test points.
  • Asphalt cured at least 7 days, SMA at least 10. Porous asphalt takes more primer: agree the quantity on site.
  • New concrete: expansion joints cut about every 5 × 6 m, 6 to 8 mm wide and at least 20 mm deep, then filled.
  • Build silicon PU between 5 and 35°C, humidity below 85%, with no rain for 4 hours. Acrylic between 10 and 35°C, humidity below 80%.
  • Concrete moisture below 8% before silicon PU goes on.

Drying

LayerSurface dryNext coat
Primer1 hour12 hours
Elastic layer1 hour3 hours
Finish layer1 hour3 hours
Line marking1 hour3 hours

At 23°C and 50% relative humidity.

FAQs

Acrylic court, in short.

Hard acrylic is primer and topcoat. Elastic acrylic adds 5 mm of coarse and fine elastic coats under the topcoat.

    Asphalt or concrete only. Oriental Yuhong does not recommend other bases.

    • Acrylic does not stop cracks in the base from coming through
    • Mix with clean water only, and not too much

    Tennis courts, low-cost outdoor basketball courts, lightweight rooftop courts and gym equipment areas.

      Yes. Supplied by Sahihi Construction Chemicals, ordered per job, ready in 3 to 5 days.

      • Send the area, the sport and the base for a written quotation